Mn0.8+x Zn0.2TixFe2-2xO4 with x=0.10, 0.15, 0.20 were prepared by conventional solid state reaction technique. Final sintering was done at 11500C for 20 hours followed by slow cooling to room temperature. To acquire desired homogeneity and phase formation samples were subjected to calcination. To establish the elemental composition EDX analysis was done. TGA, DSC and DTA were used to study the thermal behaviour of the samples.
[Satheesh D J, Reenu Jacob,Vasudevan Nair N, Jayakumari Isac (2015); Thermal Analysis of Titanium Doped Manganese Zinc Ferrite, Mn0.8+x Zn0.2TixFe2-2xO4 with x=0.10, 0.15, 0.20 Int. J. of Adv. Res. 3 (Sep). 1506-1515] (ISSN 2320-5407). www.journalijar.com
Dr. Jayakumari Isac