Abstract

Additional strengthening of superalloy N07080 described in this work was achieved by warm rolling. Control of the ratio of strength and ductile properties of the superalloy is possible by appropriate selection of the amount of warm deformation and the appropriate selection of the partial recrystallization temperature. In addition, recrystallization annealing makes it possible to equalize the grain size across the cross section of the warm rolled bars, which before recrystallization differ significantly in size in the central and peripheral parts of the bars.

Keywords

How to Cite This Article

Omer Beganovic, Belma Fakic and Branka Muminovic (2021); INFLUENCE OF WARM ROLLING AND RECRYSTALLIZATION ANNEALING ON MECHANICAL AND METALLOGRAPHIC PROPERTIES OF THE SUPERALLOY N07080, International Journal of Advanced Research (IJAR), 9 (10), 680-689, ISSN 2320-5407. DOI: https://doi.org/10.21474/IJAR01/13594

Corresponding Author

Dr. Omer Beganovic
UNIVERSITY OF ZENICA

Article Analytics

Similar Articles